中文摘要: 摘要: 广西某低品位难选铅锌矿含铅0.61%,含锌2.61%,选厂采用铅、锌各一粗两扫四精优先浮选工艺流程,因生产过程中,流程容易波动,影响铅锌浮选指标。为给现场工艺流程优化改造提供依据,在工艺矿物学研究的基础上,对该矿石进行了选矿优化试验研究。试验结果表明:在原矿磨矿细度不变的条件下,通过优化铅锌的药剂制度,并对锌中矿进行再磨,闭路试验可获得铅精矿含铅52.78%,铅回收率43.36%,锌精矿含锌50.49%,锌回收率为86.50%。相比现场生产指标,铅精矿品位提高了7.67%,铅回收率提高了10.92%,锌回收率提高了4.35%,铅锌浮选指标得到了明显改善。
Abstract:Abstract: Guangxi a low-grade lead-zinc sulfide ore contains 0.61% Pb, 2.52% Zn. The production operation of Concentrator is unstable and the phenomenon of flotation fluctuates greatly, which lead to bad lead-zinc production index. In order to provide basis for transformation of on-site process, based on the process mineralogy of the ore, the beneficiation optimization test was conducted. The results showed that lead concentrate contains 52.78% Pb with recovery of 43.36%, Zinc concentrate contains 50.49% Zn with recovery of 86.50% can be obtained through the optimization of flotation reagent system and regrinding the Zinc middling by the same grinding fineness of ROM. Compared with on-site process, the Pb grade and recovery of Lead concentrate increased by 7.67% and 10.92%, the recovery of Zinc concentrate increased by 4.35%. The flotation index of this lead-zinc ore have improved significantly.
文章编号: 中图分类号: 文献标志码:
基金项目:广东省科学院科研平台建设项目(2016GDASPT-0204)、(2016GDASPT-0307)
作者 | 单位 | |
陈志强 | 广东省资源综合利用研究所 | qaing6399@163.com |
刘超* | 广东省资源综合利用研究所 | courage0128@163.com |
罗传胜 | ||
饶金山 | ||
胡红喜 |
引用文本:
陈志强,刘超,罗传胜,饶金山,胡红喜.广西某低品位铅锌硫化矿选矿工艺优化研究[J].有色金属(选矿部分),2018(4):29-34.
ChenZhiqiang,Liuchao,罗传胜,饶金山,胡红喜.Tests of Beneficiation Optimization for a Low-Grade Lead-Zinc Sulfide Ore in Guangxi[J].Nonferrous Metals(Mineral Processing Section),2018(4):29-34.
陈志强,刘超,罗传胜,饶金山,胡红喜.广西某低品位铅锌硫化矿选矿工艺优化研究[J].有色金属(选矿部分),2018(4):29-34.
ChenZhiqiang,Liuchao,罗传胜,饶金山,胡红喜.Tests of Beneficiation Optimization for a Low-Grade Lead-Zinc Sulfide Ore in Guangxi[J].Nonferrous Metals(Mineral Processing Section),2018(4):29-34.